Free Exam: Phase 102 Product Knowledge Training
Number of Questions in Test: 127
Number of Questions in Preview: 5
Register to view all questions.
Note: Answers are not shown below but will be copied with this test.
Copy this test to my quiz maker account
Register with ClassMarker to copy free tests to give to your Test takers.
Register nowQuestion 1
A Plasma cutter works on all electrically non-conductive metals.
Type: | True/False |
Points: | 1 |
Question 2
AC stick and AC wire feed welding is least desirable because the arc is very erratic and unstable due to the current switching from positive to negative.
Type: | True/False |
Points: | 1 |
Question 3
DC is created by converting AC current into DC current. DC is the much-preferred type of current to use for welding because the arc is very rough and unstable with minimal spatter of the filler metal.
Type: | True/False |
Points: | 1 |
Question 4
[img]http://mule.ssc.tsc/pls/portal/docs/PAGE/THEMULE/DEPARTMENTS_PAGE/HR_PAGE/TRAINING_EDUCATION/OPERATIONS_TRAINING_AND_EDUCATION_PAGE/TEAM_MEMBER_TRAINING_PAGE/FRONT_PAGE_TRAINING_NEWS_ARCHIVES_PAGE/SHIELDING%20GAS%20BOTTLE.JPG[/img]
Shielding gas is a mix of 75% Argon and 25% CO2 (C-25), 100% straight Argon for aluminum, and a mixture of Argon, CO2, and helium for stainless steel (also called "tri-mix").
Shielding gas is a mix of 75% Argon and 25% CO2 (C-25), 100% straight Argon for aluminum, and a mixture of Argon, CO2, and helium for stainless steel (also called "tri-mix").
Type: | True/False |
Points: | 1 |
Question 5
Flux is a material included in a welding stick or fluxcored wire that gives off a gas when it burns and this gas serves to shield the welding arc.
Type: | True/False |
Points: | 1 |